Analysis and solution of common problems in blowing film (3 (injection molding products)
2023 11/30
Reason 1: film thickness is not uniform;
Reason 2: The cooling effect is not enough;
Reason 3: The blowing ratio is too large, causing the membrane bubble to be unstable, swinging around and back, and easy to wrinkle;
Reason 4: The Angle of the herringbone splint is too large, the membrane bubble is flattened in a short distance, so the film is also prone to wrinkle;
Reason 5: The pressure on both sides of the traction roller is inconsistent, one side is high and the other is low;
Reason 6, the axis between the guide rollers is not parallel, affecting the stability and malleability of the film, resulting in wrinkles.
solution
① Adjust the thickness of the film to ensure uniform thickness;
② Improve the cooling effect to ensure that the film can be fully cooled;
(3) Appropriately reduce the blowing ratio;
④ Properly reduce the Angle of the herringbone splint;
⑤ Adjust the pressure of the traction roller to ensure the uniform force of the film;
⑥ Check the axes of each guide axis and make them parallel to each other.